100nm Amine Gold Nanoparticles,3Kda PEG Linker
100nm_Amine_Gold_Nanoparticles_3Kda_PEG_Linker
Properties
Core Size: 100nm 
Adsorption max: 572nm 
OD per ml: 50 (50x more concentrated than our non-functionalized gold nanoparticles)
Particles per ml: 1.92E+11
Composition: Amine gold nanoparticles
Numberof Amine Groups on Surface: ~0.04/nm2
Formulation: Supplied in USP grade purified water 
Store product away from direct sunlight at 4°C. Do NOT freeze

Catalog Number Molecular weight in Daltons Pack size
RN-Au-A3K-100-25-0.5ml 3000 0.5ml
RN-Au-A3K-100-50-1ml 3000 1ml

Diameter Peak SPR Wavelength (nm) NPS/ml Wt. Conc (mg/ml) Molar Ext (M-1cm-1) Size Dispersity (+/- nm) Particle Volume (nm3) Surface Area (nm2) Surface/ Volume Ratio Particle Mass (g) Molar Mass (g/mol) Molar Concentration
100 572 1.92E+11 1.95E+00 1.57E+11 <8% 5.24E+05 3.14E+04 0.06 1.02E-14 6.11E+09 3.19E-10