designed to deliver the Purest
30nm Amine Gold Nanoparticles,5Kda PEG Linker
 30nm_Amine_Gold_Nanoparticles_3Kda_PEG_Linker
Properties
Core Size: 30nm 
Purity:<95%
Adsorption max: 526nm 
OD per ml: 50 (50x more concentrated than our non-functionalized gold nanoparticles)
Particles per ml: 8.96E+12
Composition: Amine gold nanoparticles
Numberof Amine Groups on Surface: ~0.04/nm2  
Formulation: Supplied in USP grade purifed water 
Store product away from direct sunlight at 4°C. Do NOT freeze

Catalog Number Molecular weight in Daltons Pack size
RN-Au-A5K-30-25-0.5ml 5000 0.5ml
RN-Au-A5K-30-50-1ml 5000 1ml

Diameter Peak SPR Wavelength (nm) NPS/ml Wt. Conc (mg/ml) Molar Ext (M-1cm-1) Size Dispersity (+/- nm) Particle Volume (nm3) Surface Area (nm2) Surface/ Volume Ratio Particle Mass (g) Molar Mass (g/mol) Molar Concentration
30 526 8.96E+12 2.46E+00

3.36E+09

<12%

1.41E+04

2.83E+03

0.2

2.74E-16

1.65E+08

1.49E-08