40nm Amine Gold Nanoparticles,5Kda PEG Linker
 40nm_Amine_Gold_Nanoparticles_3Kda_PEG_Linker
Properties
Core Size: 40nm 
Purity:<95%
Adsorption max: 530nm 
OD per ml: 50 (50x more concentrated than our non-functionalized gold nanoparticles)
Particles per ml: 3.58E+12
Composition: Amine gold nanoparticles
Numberof Amine Groups on Surface: ~0.04/nm2  
Formulation: Supplied in USP grade purified water 
Store product away from direct sunlight at 4°C. Do NOT freeze

Catalog Number Molecular weight in Daltons Pack size
RN-Au-A5K-40-25-0.5ml 5000 0.5ml
RN-Au-A5K-40-50-1ml 5000 1ml

Diameter Peak SPR Wavelength (nm) NPS/ml Wt. Conc (mg/ml) Molar Ext (M-1cm-1) Size Dispersity (+/- nm) Particle Volume (nm3) Surface Area (nm2) Surface/ Volume Ratio Particle Mass (g) Molar Mass (g/mol) Molar Concentration
40 530 3.58E+12

2.33E+00

8.42E+09

<12%

3.35E+04

5.03E+03

0.15

6.50E-16

3.91E+08

5.94E-09