designed to deliver the Purest
70nm Amine Gold Nanoparticles,3Kda PEG Linker
70nm_Amine_Gold_Nanoparticles_3Kda_PEG_Linker
Properties
Core Size: 70nm 
Purity:<95%
Adsorption max: 548nm 
OD per ml: 50 (50x more concentrated than our non-functionalized gold nanoparticles)
Particles per ml: 6.00E+11
Composition: Amine gold nanoparticles
Numberof Amine Groups on Surface: ~0.04/nm2  
Store product away from direct sunlight at 4°C. Do NOT freeze

Catalog Number Molecular weight in Daltons Pack size
RN-Au-A3K-70-25-0.5ml 3000 0.5ml
RN-Au-A3K-70-50-1ml 3000 1ml

Diameter Peak SPR Wavelength (nm) NPS/ml Wt. Conc (mg/ml) Molar Ext (M-1cm-1) Size Dispersity (+/- nm) Particle Volume (nm3) Surface Area (nm2) Surface/ Volume Ratio Particle Mass (g) Molar Mass (g/mol) Molar Concentration
70 548 6.00E+11 2.09E+00 5.03E+10 <10%

1.80E+05

1.54E+04

0.08571

3.48E-15

2.10E+09

9.95E-10

Reinste.com
Diagnostic Supplier