Gold Nanoparticle Conjugation Optimization Kit,15nm
Properties
Standard gold nanoparticles (100 ml, conc. OD1) 12 conjugation optimization buffers (1.5 ml each) 10% NaCl (100 ml) Protein resuspension buffer Detailed conjugation optimization protocol
Diameter | Peak SPR Wavelength (nm) | NPS/ml | Wt. Conc (mg/ml) | Molar Ext (M-1cm-1) | Size Dispersity (+/- nm) | Particle Volume (nm3) | Surface Area (nm2) | Surface/ Volume Ratio | Particle Mass (g) | Molar Mass (g/mol) | Molar Concentration |
15 | 520 | 1.64E+12 | 5.61E-02 | 3.67E+08 | <12% | 1.77E+03 | 7.07E+02 | 0.4 | 3.43E-17 | 2.06E+07 | 2.72E-09 |
Catalog Number | Particle Size in nm | Pack size in ml |
RN-Au-OptKit-15-100 | 15 nm | 100 ml |