designed to deliver the Purest
Gold Nanoparticle Conjugation Optimization Kit,40nm
Properties
Standard gold nanoparticles (100 ml, conc. OD1)
12 conjugation optimization buffers (1.5 ml each)
10% NaCl (100 ml)
Protein resuspension buffer
Detailed conjugation optimization protocol
Gold_Nanoparticle_Conjugation_Optimization_Kit_40nm

Diameter Peak SPR Wavelength (nm) NPS/ml Wt. Conc (mg/ml) Molar Ext (M-1cm-1) Size Dispersity (+/- nm) Particle Volume (nm3) Surface Area (nm2) Surface/ Volume Ratio Particle Mass (g) Molar Mass (g/mol) Molar Concentration
40 530 7.15E+10 4.65E-02 8.42E+09 <12% 3.35E+04 5.03+03 0.15 6.50E-16 3.91E+08 1.19E-10


Catalog Number Particle Size in nm Pack size in ml
RN-Au-OptKit-40-100 40 nm 100 ml