Gold Nanoparticle Conjugation Optimization Kit,80nm
Properties
Standard gold nanoparticles (100 ml, conc. OD1) 12 conjugation optimization buffers (1.5ml each) 10% NaCl (100 ml) Protein resuspension buffer Detailed conjugation optimization protocol
Diameter | Peak SPR Wavelength (nm) | NPS/ml | Wt. Conc (mg/ml) | Molar Ext (M-1cm-1) | Size Dispersity (+/- nm) | Particle Volume (nm3) | Surface Area (nm2) | Surface/ Volume Ratio | Particle Mass (g) | Molar Mass (g/mol) | Molar Concentration |
80 | 553 | 7.82E+09 | 4.06E-02 | 7.70E+10 | <10% | 2.68E+05 | 2.01E+04 | 0.075 | 5.20E-15 | 3.13E+09 | 1.30E-11 |
Catalog Number | Particle Size in nm | Pack size in ml |
RN-Au-OptKit-80-100 | 80 nm | 100 ml |