Gold Nanoparticle Conjugation Optimization Kit,10nm
Properties
Size 10 nm Standard gold nanoparticles (100 ml, conc. OD1) 12 conjugation optimization buffers (1.5 ml each) 10% NaCl (100 ml) Protein resuspension buffer Detailed conjugation optimization protocol

Diameter | Peak SPR Wavelength (nm) | NPS/ml | Wt. Conc (mg/ml) | Molar Ext (M-1cm-1) | Size Dispersity (+/- nm) | Particle Volume (nm3) | Surface Area (nm2) | Surface/ Volume Ratio | Particle Mass (g) | Molar Mass (g/mol) | Molar Concentration |
10 | 515-520 | 5.98E+12 | 6.07E-02 | 1.01E+08 | <15% | 5.24E+02 | 3.14E+02 | 0.6 | 1.02E-17 | 6.11E+06 | 9.93E-09 |
Catalog Number | Particle Size in nm | Pack size in ml |
RN-Au-OptKit-10-100 | 10 nm | 100 ml |