designed to deliver the Purest
Gold Nanoparticle Conjugation Optimization Kit,30nm
Properties
Standard gold nanoparticles (100 ml, conc. OD1)
12 conjugation optimization buffers (1.5 ml each)
10% NaCl (100 ml)
Protein resuspension buffer
Detailed conjugation optimization protocol
Gold_Nanoparticle_Conjugation_Optimization_Kit_30nm

Diameter Peak SPR Wavelength (nm) NPS/ml Wt. Conc (mg/ml) Molar Ext (M-1cm-1) Size Dispersity (+/- nm) Particle Volume (nm3) Surface Area (nm2) Surface/ Volume Ratio Particle Mass (g) Molar Mass (g/mol) Molar Concentration
30 526 1.79E+11 4.91E-02 3.36E+09 <12% 1.41E+04 2.83E+03 0.2 2.74E-16 1.65E+08 2.98E-10


Catalog Number Particle Size in nm Pack size in ml
RN-Au-OptKit-30-100 30 nm 100 ml

Reinste.com
Diagnostic Supplier