Gold Nanoparticle Conjugation Optimization Kit,70nm
Properties
Standard gold nanoparticles (100 ml, conc. OD1) 12 conjugation optimization buffers (1.5 ml each) 10% NaCl (100 ml) Protein resuspension buffer Detailed conjugation optimization protocol
![Gold_Nanoparticle_Conjugation_Optimization_Kit_70nm Gold_Nanoparticle_Conjugation_Optimization_Kit_70nm](Image/Gold_Nanoparticle_Conjugation_Optimization_Kit_70nm.jpg)
Diameter | Peak SPR Wavelength (nm) | NPS/ml | Wt. Conc (mg/ml) | Molar Ext (M-1cm-1) | Size Dispersity (+/- nm) | Particle Volume (nm3) | Surface Area (nm2) | Surface/ Volume Ratio | Particle Mass (g) | Molar Mass (g/mol) | Molar Concentration |
70 | 548 | 1.20E+10 | 4.17E-02 | 5.03E+10 | <10% | 1.80E+05 | 1.54E+04 | 0.086 | 3.48E-15 | 2.10E+09 | 1.99E-11 |
Catalog Number | Particle Size in nm | Pack size in ml |
RN-Au-OptKit-70-100 | 70 nm | 100 ml |