Properties
Gold nanoparticle core Size: 15 nm Optical density: 3OD (conc. 4.92E+12 particles/ml) Conjugated protein: Streptavidin from Streptomyces avidinii Working dilution: 1:25-1:100 Supplied in: 0.01M PBS (pH 7.4) 20% glycerol (v/v), 1% BSA and 15mM sodium azide
CATALOG NUMBER PACK SIZE
RN-Au-C-15-Streptavidin-1ml | 1 ml |
Diameter | Peak SPR Wavelength (nm) | NPS/ml | Wt. Conc (mg/ml) | Molar Ext (M-1cm-1) | Size Dispersity (+/- nm) | Particle Volume (nm3) | Surface Area (nm2) | Surface/ Volume Ratio | Particle Mass (g) | Molar Mass (g/mol) | Molar Concentration |
15 | 520 | 4.92E+12 | 1.68E-01 | 3.67E+08 | <12% | 1.77E+03 | 7.07E+02 | 0.4 | 3.43E-17 | 2.06E+07 | 8.16E-09 |