10nm Amine Gold Nanoparticles,5Kda PEG Linker
 5nm_Amine_Gold_Nanoparticles_3Kda_PEG_Linker
Properties
Core Size: 10nm 
Purity:<95%
Adsorption max: 520nm 
Composition: Amine gold nanoparticles
OD per ml: 50 (50x more concentrated than our non-functionalized gold nanoparticles)
Particles per ml: 2.99E+14
Numberof Amine Groups on Surface: ~0.04/nm2  
Formulation: Supplied in USP grade purified water 
Store product away from direct sunlight at 4°C. Do NOT freeze

Catalog Number Molecular weight in Daltons Pack size
RN-Au-A5K-10-25-0.5ml 5000 0.5ml
RN-Au-A5K-10-50-1ml 5000 1ml

Diameter Peak SPR Wavelength (nm) NPS/ml Wt. Conc (mg/ml) Molar Ext (M-1cm-1) Size Dispersity (+/- nm) Particle Volume (nm3) Surface Area (nm2) Surface/ Volume Ratio Particle Mass (g) Molar Mass (g/mol) Molar Concentration
10 515-520 2.99E+14 3.04E+00 1.10E+07 <15% 5.24E+02 3.14E+02 0.6

1.02E-17

6.11E+06 4.97E-07