30nm Carboxyl Gold Nanoparticles,5kDa PEG linker
Properties
Core Size: 30nm Purity:<95% Adsorption max: 526nm OD per ml: 50 (50x more concentrated than our non-functionalized gold nanoparticles) Particles per ml: 8.96E+12 Composition: Carboxyl gold nanoparticles Numberof Carboxyl Groups on Surface: ~0.04/nm2 Formulation: Supplied in USP grade purifed water Store product away from direct sunlight at 4°C. Do NOT freeze
Catalog Number | Molecular weight in Daltons | Pack size |
CGC5K-30-25 | 5000 | 0.5ml |
CGC5K-30-25 | 5000 | 1ml |
Diameter | Peak SPR Wavelength (nm) | NPS/ml | Wt. Conc (mg/ml) | Molar Ext (M-1cm-1) | Size Dispersity (+/- nm) | Particle Volume (nm3) | Surface Area (nm2) | Surface/ Volume Ratio | Particle Mass (g) | Molar Mass (g/mol) | Molar Concentration |
30 | 526 | 8.96E+12 | 2.46E+00 | 3.36E+09 | <12% | 1.41E+04 | 2.83E+03 | 0.2 | 2.74E-16 | 1.65E+08 | 1.49E-08 |