40nm Amine Gold Nanoparticles,3Kda PEG Linker
Properties
Core Size: 40nm Purity:<95% Adsorption max: 530nm OD per ml: 50 (50x more concentrated than our non-functionalized gold nanoparticles) Particles per ml: 3.58E+12 Composition: Amine gold nanoparticles Numberof Amine Groups on Surface: ~0.04/nm2 Formulation: Supplied in USP grade purified water Store product away from direct sunlight at 4°C. Do NOT freeze
Catalog Number | Molecular weight in Daltons | Pack size |
RN-Au-A3K-40-25-0.5ml | 3000 | 0.5ml |
RN-Au-A3K-40-50-1ml | 3000 | 1ml |
Diameter | Peak SPR Wavelength (nm) | NPS/ml | Wt. Conc (mg/ml) | Molar Ext (M-1cm-1) | Size Dispersity (+/- nm) | Particle Volume (nm3) | Surface Area (nm2) | Surface/ Volume Ratio | Particle Mass (g) | Molar Mass (g/mol) | Molar Concentration |
40 | 530 | 3.58E+12 | 2.33E+00 |
8.42E+09 |
<12% | 3.35E+04 |
5.03E+03 |
0.15 | 6.50E-16 |
3.91E+08 |
5.94E-09 |