5nm Amine Gold Nanoparticles,3Kda PEG Linker
Properties
Core Size: 5nm Purity:<95% Adsorption max: 515-520nm Composition: Amine gold nanoparticles OD per ml: 50 (50x more concentrated than our non-functionalized gold nanoparticles) Particles per ml: 2.73E+15 Numberof Amine Groups on Surface: ~0.04/nm2 Formulation: Supplied in USP grade purified water Store product away from direct sunlight at 4°C. Do NOT freeze
Catalog Number | Molecular weight in Daltons | Pack size |
RN-Au-A3K-5-25-0.5ml | 3000 | 0.5ml |
RN-Au-A3K-5-50-1ml | 3000 | 1ml |
Diameter | Peak SPR Wavelength (nm) | NPS/ml | Wt. Conc (mg/ml) | Molar Ext (M-1cm-1) | Size Dispersity (+/- nm) | Particle Volume (nm3) | Surface Area (nm2) | Surface/ Volume Ratio | Particle Mass (g) | Molar Mass (g/mol) | Molar Concentration |
5 | 515-520 | 2.74E+15 | 3.47E+00 | 1.10E+07 | <15% | 6.54E+01 | 7.85E+01 | 1.2 | 1.27E-18 | 7.64E+05 | 4.54E-06 |