70nm Carboxyl Gold Nanoparticles,3kDa PEG linker
Properties
Core Size: 70nm Purity:<95% Adsorption max: 548nm OD per ml: 50 (50x more concentrated than our non-functionalized gold nanoparticles) Particles per ml: 6.00E+11 Composition: Carboxyl gold nanoparticles Numberof Carboxyl Groups on Surface: ~0.04/nm2 Store product away from direct sunlight at 4°C. Do NOT freeze
Catalog Number | Molecular weight in Daltons | Pack size |
CGC3K-70-25 | 3000 | 0.5ml |
CGC3K-70-50 | 3000 | 1ml |
Diameter | Peak SPR Wavelength (nm) | NPS/ml | Wt. Conc (mg/ml) | Molar Ext (M-1cm-1) | Size Dispersity (+/- nm) | Particle Volume (nm3) | Surface Area (nm2) | Surface/ Volume Ratio | Particle Mass (g) | Molar Mass (g/mol) | Molar Concentration |
60 | 540 | 6.00E+11 | 2.09E+00 | 5.03E+10 | <10% | 1.80E+05 |
1.54E+04 | 0.08571 |
3.48E-15 | 2.10E+09 | 9.95E-10 |