Gold Nanoparticle Conjugation Optimization Kit,100nm
Properties
Gold Nanoparticle Conjugation Optimization Kit, Size 100 nm Standard gold nanoparticles (100 ml, conc. OD1) 12 conjugation optimization buffers (1.5 ml each) 10% NaCl (100ml) Protein resuspension buffer Detailed conjugation optimization protocol
Diameter | Peak SPR Wavelength (nm) | NPS/ml | Wt. Conc (mg/ml) | Molar Ext (M-1cm-1) | Size Dispersity (+/- nm) | Particle Volume (nm3) | Surface Area (nm2) | Surface/ Volume Ratio | Particle Mass (g) | Molar Mass (g/mol) | Molar Concentration |
100 | 553 | 3.84E+09 | 3.89E-02 | 1.57E+11 | <8% | 5.24E+05 | 3.14E+04 | 0.06 | 1.02E-14 | 6.11E+09 | 6.37E-12 |
Catalog Number | Particle Size in nm | Pack size in ml |
RN-Au-OptKit-100-100 | 100 nm | 100 ml |