Gold Nanoparticle Conjugation Optimization Kit,5nm
Properties
Size 5 nm Standard gold nanoparticles (100ml, conc. OD1) 12 conjugation optimization buffers (1.5ml each) 10% NaCl (100ml) Protein resuspension buffer Detailed conjugation optimization protocol
Diameter | Peak SPR Wavelength (nm) | NPS/ml | Wt. Conc (mg/ml) | Molar Ext (M-1cm-1) | Size Dispersity (+/- nm) | Particle Volume (nm3) | Surface Area (nm2) | Surface/ Volume Ratio | Particle Mass (g) | Molar Mass (g/mol) | Molar Concentration |
20 | 515-520 | 5.47E+13 | 6.94E-02 | 1.10E+07 | <15% | 6.54E+01 | 7.85E+01 | 1.2 | 1.27E-18 | 7.64E+05 | 9.08E-08 |
Catalog Number | Particle Size in nm | Pack size in ml |
RN-Au-OptKit-5-100 | 5 nm | 100 ml |