Protein A - 15 nm Gold Conjugate
Properties
Gold nanoparticle core size: 15 nm Optical density: 3OD (conc. 4.92E+12 particles/ml) Conjugated protein: Protein A, from S. aureus Working dilution: 1:25-1:100 Supplied in: 0.01M PBS (pH 7.4), 20% glycerol (v/v), 1% BSA and 15mM sodium azide
CATALOG NUMBER PACK SIZE
RN-Au-C-15-Protein A-1ml | 1 ml |
Diameter | Peak SPR Wavelength (nm) | NPS/ml | Wt. Conc (mg/ml) | Molar Ext (M-1cm-1) | Size Dispersity (+/- nm) | Particle Volume (nm3) | Surface Area (nm2) | Surface/ Volume Ratio | Particle Mass (g) | Molar Mass (g/mol) | Molar Concentration |
15 | 515-520 | 1.79E+13 | 1.82E-01 | 1.01E+08 | <15% | 5.24E+02 | 3.14E+02 | 0.06 | 1.02E-17 | 6.11E+06 | 2.98E-08 |